The surface irregularirites of electrodes used in an electrochmical machining (ECM) process are 3 μm and 6 μm as shown in the figure. If the work-piece is of pure iron and 12V DC is applied between the electrodes, the largest feed rate is mm/min Conductivity of the electrolyte 0.02 ohm−1mm−1 Over-potential volate 1.5 V Density of iron 7860 kg/m3 Atomic weight of iron 55.85 gm Assume the iron to be dissolved as Fe+2 and the Faraday constant to be 96500 Coulomb.

Answer» The surface irregularirites of electrodes used in an electrochmical machining (ECM) process are 3 μm and 6 μm as shown in the figure. If the work-piece is of pure iron and 12V DC is applied between the electrodes, the largest feed rate is mm/min



















Conductivity of the electrolyte 0.02 ohm1mm1
Over-potential volate 1.5 V
Density of iron 7860 kg/m3
Atomic weight of iron 55.85 gm

Assume the iron to be dissolved as Fe+2 and the Faraday constant to be 96500 Coulomb.