1.

The tensile properties of a low-pressure plasma-deposited nickel-base superalloy from ____________(a) 25 to 100° C(b) 250 to 1010° C(c) 25 to 1010° C(d) 100 to 250° CThe question was posed to me in an interview for job.This interesting question is from Ring Tension Test in portion Testing of Concrete of Concrete Technology

Answer»

Right OPTION is (c) 25 to 1010° C

Easy explanation: A ring tensile TEST USING a split disc fixture was developed and used to evaluate the tensile PROPERTIES of a low-pressure plasma-deposited nickel-base superalloy from 25 to 1010° C.