| 1. |
To produce the smoked rubber, the rubber sheets are hanged in smoked chambers at __________(a) 10-20^oC(b) 20-30^oC(c) 30-40^oC(d) 40-50^oCThe question was asked during an interview.This interesting question is from Natural Rubber topic in portion High Polymers and Plastics of Applied Chemistry |
|
Answer» The correct answer is (d) 40-50^oC |
|