1.

Out of C and CO which is a better reducing agent for FeO : In the lower part of blast furnace (Higher temperature).

Answer»

SOLUTION :In the lower part of blast furnace i.e., at higher temperature, C is a better reducing AGENT because the CURVE of `C to CO_(2)` lies below the curve for `2Fe+O_(2) to 2FeO`.