Roasted copper pyrite on smelting with sand produces |
|
Answer» `FeSiO_3` as fusible SLAG and `Cu_2 S` as matte `FeO + UNDERSET("Silica")(SiO_2) to underset("(slag)")underset("Ferrous silicate")(FeSiO_3)` |
|