Stress-corrosion cracking occurs due to the simultaneous presence of tensile stress and a specific corrosive medium.(a) True(b) FalseThis question was posed to me in a job interview.Question is taken from Eight Forms topic in section Eight Forms of Corrosion of Corrosion Engineering

Answer»

The correct choice is (a) True

Explanation: STRESS–corrosion cracking occurs DUE to the simultaneous PRESENCE of tensile stress either is caused by residual or external stress and a specific corrosive medium. Residual stress is caused due to WELDING, cold working, etc.